Bitumen Specification Viscosity Grade Analysis

(V.G 30)

Specification Acceptable Range Test Method Explanations
Absolute Viscosity Min 2400  ASTM – D4402 at 60° c, Poises
Kinematic Viscosity Min 350 ASTM – D4402 at 135° c, c.st
Solubility 99.0 Min ASTM – D2042 in CCL4, %
Flash Point 220 Min ASTM – D92 ° c
Penetration 50 – 70 ASTM – D5 at 25° c, mm/10
Softening Point Min 47 ASTM – D36 ° c
Test on Reside Form Thin Film Oven Test (T.F.O.T.)
Ratio Viscosity Max 4.0 ASTM – D4402 at 60° c, %
Ductility Min 40 ASTM – D113 at 25° c, cm

(V.G 40)

Specification Acceptable Range Test Method Explanations
Absolute Viscosity Min 3200  ASTM – D4402 at 60° c, Poises
Kinematic Viscosity Min 400 ASTM – D4402 at 135° c, c.st
Solubility 99.0 Min ASTM – D2042 in CCL4, %
Flash Point 220 Min ASTM – D92 ° c
Penetration 40 – 60 ASTM – D5 at 25° c, mm/10
Softening Point Min 50 ASTM – D36 ° c
Test on Reside Form Thin Film Oven Test (T.F.O.T.)
Ratio Viscosity Max 4.0 ASTM – D4402 at 60° c, %
Ductility Min 25 ASTM – D113 at 25° c, cm

(60/70)

Specification Acceptable Range Test Method Explanations
Penetration 60 -70 ASTM – D5 at 25° c, mm/10
Softening Point 46 Min ASTM – D36 ° c
Ductility 100 Min ASTM – D113 at 25° c, cm
Solubility 99.0 Min ASTM – D2024 in CCL4, %
Specific Gravity 1.01 – 1.06 ASTM – D70 at 25° c
Spot Test Negative T102 in Naphtha
Flash Point 250 Min ASTM – D92 ° c
Test on Reside Form Thin Film Oven Test (T.F.O.T.)
Drop in Penetration 20 Max ASTM – D5 & D6 %
Mass Loss 0.2 Max ASTM – D6 Wt%

(80/100)

Specification Acceptable Range Test Method Explanations
Penetration 80 -100 ASTM – D5 at 25° c, mm/10
Softening Point 42 Min ASTM – D36 ° c
Ductility 100 Min ASTM – D113 at 25° c, cm
Solubility 99.0 Min ASTM – D2024 in CCL4, %
Specific Gravity 1.01 – 1.06 ASTM – D70 at 25° c
Spot Test Negative T102 in Naphtha
Flash Point 250 Min ASTM – D92 ° c
Test on Reside Form Thin Film Oven Test (T.F.O.T.)
Drop in Penetration 20 Max ASTM – D5 & D6 %
Mass Loss 0.2 Max ASTM – D6 Wt%